  3. Newsgroups: sci.materials
  4. Subject: Re: Need to make a glass surface rough ...
  5. Message-ID: <1992Dec27.093111.2304@ucbeh.san.uc.edu>
  6. Date: 27 Dec 92 09:31:11 EST
  7. References: <4rlrf7c@lynx.unm.edu> <6rlracd@lynx.unm.edu>
  8. Followup-To: swami@chtm.eece.unm.edu, swami@triton.unm.edu,sci.materials
  9. Distribution: world
  10. Organization: Univ. of Cincinnati
  11. Lines: 11
  12.  
  13. In article <6rlracd@lynx.unm.edu>, swami@chtm.eece.unm.edu (Swami srinivasan) 
  14. writes:
  15. > I need to make a 50 microns x 1000 microns section of glass surface
  16. > ROUGH. I have  a mask with the required dimensions. Most etchants are
  17. ... the purpose was to make a defusive area, ...... 
  18.  
  19. Could you deposit something on the surface to make it defusive?  For example,
  20. some Si.